高熵合金的低温塑性变形机制及强韧化研究进展 |
| 刘俊鹏, 陈浩, 张弛, 杨志刚, 张勇, 戴兰宏 |
|
Progress of Cryogenic Deformation and Strengthening-Toughening Mechanisms of High-Entropy Alloys |
| LIU Junpeng, CHEN Hao, ZHANG Chi, YANG Zhigang, ZHANG Yong, DAI Lanhong |
| 图10 Fe55Co17.5Cr12.5Ni10Mo3C2高熵合金的微观形貌、力学性能及低温组织演变特征[ Color online (a) TEM image and SAED patterns of the M6C (inset A) and M23C6 (inset B) precipitates in the original sample (b) tensile properties at room and cryogenic temperatures (c) EBSD images of HEA alloy during the tensile test at 77 K (εT—true strain) |
| Fig.10 Morphology, mechanical properties, and microstructure evolutions of Fe55Co17.5Cr12.5Ni10Mo3C2 HEA[ |
|