高熵合金的低温塑性变形机制及强韧化研究进展 |
| 刘俊鹏, 陈浩, 张弛, 杨志刚, 张勇, 戴兰宏 |
|
Progress of Cryogenic Deformation and Strengthening-Toughening Mechanisms of High-Entropy Alloys |
| LIU Junpeng, CHEN Hao, ZHANG Chi, YANG Zhigang, ZHANG Yong, DAI Lanhong |
| 图9 铁基中熵合金的低温硬化机制示意图[ Color online |
| Fig.9 Schematic diagram of cryogenic work-hardening mechanisms in Fe-based medium-entropy alloy (GB—grain boundary, SB—shear band)[ |
|