高熵合金的低温塑性变形机制及强韧化研究进展 |
| 刘俊鹏, 陈浩, 张弛, 杨志刚, 张勇, 戴兰宏 |
|
Progress of Cryogenic Deformation and Strengthening-Toughening Mechanisms of High-Entropy Alloys |
| LIU Junpeng, CHEN Hao, ZHANG Chi, YANG Zhigang, ZHANG Yong, DAI Lanhong |
| 图1 具有严重晶格畸变特征的高熵合金化学无序原子结构示意图[ Color online |
| Fig.1 Schematic of crystal structure in high-entropy alloy (HEA) with severe distortion[ |
|