冷喷涂辅助感应重熔合成AlCo x CrFeNiCu高熵合金涂层的显微组织和性能 |
||||||||||||||||||
| 冯力, 王贵平, 马凯, 杨伟杰, 安国升, 李文生 | ||||||||||||||||||
|
Microstructure and Properties of AlCo x CrFeNiCu High-Entropy Alloy Coating Synthesized by Cold Spraying Assisted Induction Remelting |
||||||||||||||||||
| FENG Li, WANG Guiping, MA Kai, YANG Weijie, AN Guosheng, LI Wensheng | ||||||||||||||||||
| 表2 AlCo x CrFeNiCu高熵合金涂层各相的晶格常数 (nm) |
||||||||||||||||||
| Table 2 Lattice constants of each phase in the AlCo x -CrFeNiCu high-entropy alloy coating |
||||||||||||||||||
|
||||||||||||||||||