冷喷涂辅助感应重熔合成AlCo x CrFeNiCu高熵合金涂层的显微组织和性能 |
| 冯力, 王贵平, 马凯, 杨伟杰, 安国升, 李文生 |
|
Microstructure and Properties of AlCo x CrFeNiCu High-Entropy Alloy Coating Synthesized by Cold Spraying Assisted Induction Remelting |
| FENG Li, WANG Guiping, MA Kai, YANG Weijie, AN Guosheng, LI Wensheng |
| 图9 AlCo x CrFeNiCu高熵合金涂层磨损形貌的SEM像 |
| Fig.9 Low (a1-e1) and high (a2-e2) magmfied SEM images showing wear morphologies of AlCo x CrFeNiCu high-entropy alloy coatings (a1, a2) x = 0 (b1, b2) x = 0.5 (c1, c2) x = 1.0 (d1, d2) x = 1.5 (e1, e2) x = 2.0 |
|