热等静压成形Inconel 718粉末合金的显微组织和力学性能 |
| 徐磊, 田晓生, 吴杰, 卢正冠, 杨锐 |
|
Microstructure and Mechanical Properties of Inconel 718 Powder Alloy Prepared by Hot Isostatic Pressing |
| XU Lei, TIAN Xiaosheng, WU Jie, LU Zhengguan, YANG Rui |
| 图8 Inconel 718粉末合金构件工业及显微CT测试结果 |
| Fig.8 Industrial computerized tomography (CT) (a) and Micro-CT (b) analyses of PM Inconel 718 alloys |
|