热等静压成形Inconel 718粉末合金的显微组织和力学性能 |
| 徐磊, 田晓生, 吴杰, 卢正冠, 杨锐 |
|
Microstructure and Mechanical Properties of Inconel 718 Powder Alloy Prepared by Hot Isostatic Pressing |
| XU Lei, TIAN Xiaosheng, WU Jie, LU Zhengguan, YANG Rui |
| 图2 Inconel 718预合金粉末粒度分布 |
| Fig.2 Differential size distributions of Inconel 718 pre-alloyed powders (D10, D50, and D90 indicate 10%, 50%, and 90% cumulative particle sizes, respectively) |
|