基于纳米活性结构的不互溶W-Cu体系直接合金化及其热力学机制 |
| 王寒玉, 李彩, 赵璨, 曾涛, 王祖敏, 黄远 |
|
Direct Alloying of Immiscible Tungsten and Copper Based on Nano Active Structure and Its Thermodynamic Mechanism |
| WANG Hanyu, LI Cai, ZHAO Can, ZENG Tao, WANG Zumin, HUANG Yuan |
| 图9 基于纳米活性结构的W-Cu直接合金化过程中的能量变化曲线 |
| Fig.9 Calculated energy curves of W-Cu direct alloying processes based on nano active structure for the W-Cu systems (Δ (a) without pressure (b) under 106 MPa pressure |
|