基于纳米活性结构的不互溶W-Cu体系直接合金化及其热力学机制 |
| 王寒玉, 李彩, 赵璨, 曾涛, 王祖敏, 黄远 |
|
Direct Alloying of Immiscible Tungsten and Copper Based on Nano Active Structure and Its Thermodynamic Mechanism |
| WANG Hanyu, LI Cai, ZHAO Can, ZENG Tao, WANG Zumin, HUANG Yuan |
| 图6 W/Cu层状复合材料的剪切断口形貌(W侧)的SEM像以及EDS分析结果 |
| Fig.6 SEM image of shear fracture surface (W side) of the W/Cu layered composite (a); EDS analysis results of the region marked with rectangles I (b), II (c), and III (d) |
|