基体表面喷丸处理对纳米晶涂层循环氧化行为的影响 |
| 黄鼎, 乔岩欣, 杨兰兰, 王金龙, 陈明辉, 朱圣龙, 王福会 |
|
Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating |
| HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui |
| 图5 1100℃下氧化0、5、20和100 cyc后抛光高温合金基体/纳米晶涂层界面微观组织及沿虚线的EDS线扫描结果 |
| Fig.5 Microstructures (left) and EDS line scanning results along the dash lines (right) of the interface between the polished substrate and nanocrystalline coating after 0 (a), 5 (b), 20 (c), and 100 (d) cyc oxidation at 1100oC |
|