基体表面喷丸处理对纳米晶涂层循环氧化行为的影响 |
| 黄鼎, 乔岩欣, 杨兰兰, 王金龙, 陈明辉, 朱圣龙, 王福会 |
|
Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating |
| HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui |
| 图4 沉积在抛光和喷丸高温合金表面上的纳米晶涂层在1100℃下100 cyc后的截面和表面形貌 |
| Fig.4 Cross-sectional (a, c) and surface (b, d) morphologies of nanocrystalline coatings deposited on polished (a, b) and shot peened (c, d) superalloys after 100 cyc at 1100oC |
|