后时效对超细晶6061铝合金微观结构与力学性能的影响 |
| 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏 |
|
Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy |
| LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong |
| 图6 不同状态下合金内部析出的演变示意图 |
| Fig.6 Schematics of the evolution of the internal precipitation of the alloy in different states Color online (a) solid-solution treatment (SST) (b) ECAPed (c) high temperature (> 110oC) post-aging after ECAP (d) low temperature (< 80oC) post-aging after ECAP |
|