后时效对超细晶6061铝合金微观结构与力学性能的影响 |
| 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏 |
|
Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy |
| LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong |
| 图1 6061铝合金不同处理态XRD谱 |
| Fig.1 XRD spectra of 6061 aluminum alloy at T6 state (a) and ECAPed and post-aged state (b) (ECAP—equal channel angular pressing, RT—room temperature) |
|