热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响 |
| 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐 |
|
Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting |
| ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui |
| 图12 不同热处理后Ti55531合金多孔材料孔梁母材压缩断裂能 |
| Fig.12 Compression fracture energies of the parent materials of porous Ti55531 specimens after different heat treatments |
|