热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响 |
| 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐 |
|
Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting |
| ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui |
| 图2 Ti55531合金多孔材料结构模型和选区激光熔化打印样品 |
| Fig.2 Porous structure models (a, b) and selective laster melting (SLM) fabricated specimen (c) of porous Ti55531 alloy |
|