含Cu马氏体时效不锈钢的组织与强韧性
王滨, 牛梦超, 王威, 姜涛, 栾军华, 杨柯

Microstructure and Strength-Toughness of a Cu-Contained Maraging Stainless Steel
WANG Bin, NIU Mengchao, WANG Wei, JIANG Tao, LUAN Junhua, YANG Ke
图9 含Cu马氏体时效不锈钢试样在480℃时效90 h后的HAADF像和EDS元素面扫描图
Fig.9 HAADF image and corresponding EDS elemental mapping of reverted austenite in the Cu-contained maraging stainless steel sample aged at 480oC for 90 h
Color online