含Cu马氏体时效不锈钢的组织与强韧性
王滨, 牛梦超, 王威, 姜涛, 栾军华, 杨柯

Microstructure and Strength-Toughness of a Cu-Contained Maraging Stainless Steel
WANG Bin, NIU Mengchao, WANG Wei, JIANG Tao, LUAN Junhua, YANG Ke
图2 含Cu马氏体时效不锈钢试样淬火态的SEM像和480℃时效0.5 h的OM像
Fig.2 SEM image of as-quanched Cu-contained maraging stainless steel sample (a) and OM image of the sample aged at 480oC for 0.5 h (b)