尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响 |
| 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆 |
|
Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting |
| HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan |
| 图11 不同尺寸效应样品的室温拉伸应力-应变曲线 |
| Fig.11 Stress-strain curves of L100 (a), T100 (b), T200 (c), and T300 (d) series samples |
|