尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响 |
| 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆 |
|
Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting |
| HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan |
| 图10 T300-L100和T300-L1000样品析出相的EBSD分析 |
| Fig.10 Phase distribution images by EBSD in SLM 304L stainless steel of T300-L100 (a) and T300-L1000 (b) Color online |
|