尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响 |
| 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆 |
|
Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting |
| HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan |
| 图8 SLM 304L不锈钢T300系列样品显微组织的OM像 |
| Fig.8 OM images of microstructures of T300 series samples in SLM 304L stainless steel (a) T300-L100 (b) T300-L500 (c) T300-700 (d) T300-L1000 |
|