尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响 |
| 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆 |
|
Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting |
| HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan |
| 图7 SLM 304L不锈钢T200系列样品显微组织的OM像 |
| Fig.7 OM images of microstructures of T200 series samples in SLM 304L stainless steel (a) T200-L100 (b) T200-L500 (c) T200-700 (d) T200-L1000 |
|