尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响 |
| 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆 |
|
Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting |
| HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan |
| 图5 不同尺寸效应SLM 304L样品沿打印构建方向显微组织的OM像 |
| Fig.5 OM images of SLM 304L stainless steel samples with different T × L sizes along the building direction (a) T1-L5 (b) T2-L5 (c) T20-L10 (d) T20-L100 (e) T20-L700 (f) T20-L1000 |
|