冷轧变形对高性能Cu-Ni-Si合金组织性能与析出行为的影响
王长胜, 付华栋, 张洪涛, 谢建新

Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys
WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin
表1 不同时效温度下合金Avrami方程系数n和b的值
Table 1 Values of coefficients n and b in Avrami equation for alloys at different aging temperatures
Deformation / %400oC450oC500oC
nbnbnb
00.476970.1968160.531490.1439920.606330.093694
650.707260.0890450.501740.1849440.661540.075043
750.594240.1226170.574030.1002210.596980.116676
850.527620.1613060.538650.1037050.537060.170424
950.669980.0885100.544470.1184760.462260.283687