冷轧变形对高性能Cu-Ni-Si合金组织性能与析出行为的影响 |
| 王长胜, 付华栋, 张洪涛, 谢建新 |
|
Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys |
| WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin |
| 图9 冷轧变形试样时效后的拉伸性能及合金性能分布[ |
| Fig.9 Engineering stress-strain curves of the alloy after aging and alloys' properties distribution (a) ε = 85%, 450oC (b) ε = 95%, 400oC (c) ε = 95%, 450oC (d) properties distribution[ |
|