冷轧变形对高性能Cu-Ni-Si合金组织性能与析出行为的影响 |
| 王长胜, 付华栋, 张洪涛, 谢建新 |
|
Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys |
| WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin |
| 图8 冷轧变形+不同温度时效后合金的硬度与导电率 |
| Fig.8 Electrical conductivities (a, c, e) and hardnesses (b, d, f) of the alloy after cold-rolling deformation and aging at different temperatures (a, b) 400oC (c, d) 450oC (e, f) 500oC |
|