冷轧变形对高性能Cu-Ni-Si合金组织性能与析出行为的影响 |
| 王长胜, 付华栋, 张洪涛, 谢建新 |
|
Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys |
| WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin |
| 图1 不同冷轧变形量下Cu-3.28Ni-0.60Si-0.22Zn-0.11Cr-0.04P合金的DSC测试结果 |
| Fig.1 DSC test results of the Cu-3.28Ni-0.60Si-0.22Zn-0.11Cr-0.04P alloy by different cold-rolling deformations (ε) (a) ε = 0% (b) ε = 65% (c) ε = 75% (d) ε = 85% (e) ε = 95% (f) precipitation temperatures and recrystallization initial temperatures |
|