Cu对Ni-Ti合金抗支架内再狭窄与耐蚀性能的影响
许林杰, 刘徽, 任玲, 杨柯

Effect of Cu on In-Stent Restenosis and Corrosion Resistance of Ni-Ti Alloy
XU Linjie, LIU Hui, REN Ling, YANG Ke
表2 从动电位极化曲线与EIS图中获得的电化学参数
Table 2 Electrochemical parameters obtained from polarization curves of driven potential and EIS diagram
AlloyEcorr / mVicorr / (nA·cm-2)Epit / mVRs / (Ω·cm2)Rc1 / (104 Ω·cm2)Qc1 / (μΩ-1·s n ·cm-2)
Ni-Ti-399 ± 6299.7 ± 13.4828 ± 3013.73 ± 1.646.41 ± 1.2052.3 ± 1.5
Ni-Ti-Cu-283 ± 5259.5 ± 16.3862 ± 2511.79 ± 1.2267.32 ± 3.4251.5 ± 1.2