表1 不同样品与去离子水、甘油和溴代萘的接触角及表面自由能测量结果
Table 1 Measurement results of contact angle and surface free energy of different samples with deionized water, glycerin, and bromonaphthalene
Alloyθ1 / (°)θ2 / (°)θ3 / (°)γsvp / (mJ·m-2)γsvd / (mJ·m-2)
Ni-Ti53.44 ± 1.9455.53 ± 3.2718.59 ± 0.3711.94 ± 1.3139.31 ± 0.83
Ni-Ti-Cu58.36 ± 3.6065.73 ± 3.5819.12 ± 0.888.99 ± 1.1237.56 ± 1.08