组元占比对层状纳米孪晶Cu力学行为的影响 |
| 万涛, 程钊, 卢磊 |
|
Effect of Component Proportion on Mechanical Behaviors of Laminated Nanotwinned Cu |
| WAN Tao, CHENG Zhao, LU Lei |
| 图4 LNT Cu拉伸变形前后侧表面高度起伏轮廓和分布曲线以及相对侧向应变(Δεy)分布 |
| Fig.4 Illustration of tensile specimen and the observed area (a), CLSM images (b1-d1, b2-d2) and corresponding average height profile (b3-d3) and average relative lateral strain (Δεy) (b4-d4) of LNT-10% (b1-b4), LNT-50% (c1-c4), and LNT-90% (d1-d4) deformed at εapp = 0 and 6%, respectively (The area closed by white dashed lines in Fig.4b2 indicates the strain localization zone. |Δε |
|