镁合金LPSO/SFs结构间{ |
| 邵晓宏, 彭珍珍, 靳千千, 马秀良 |
|
Unravelling the { |
| SHAO Xiaohong, PENG Zhenzhen, JIN Qianqian, MA Xiuliang |
| 图9 LPSO结构扭折促进{ |
| Fig.9 Atomic-resolution HAADF-STEM image of TB connecting with KB between LPSO structures, where the twinning just nucleated in the left side of the kink (a), and nearly occupied the left side of the kink (b) (LTB—left twin boundary, RTB—right twin boundary, CTB—coherent twin boundary) |
|