镁合金LPSO/SFs结构间{}孪晶交汇机制的原子尺度研究
|
|
邵晓宏, 彭珍珍, 靳千千, 马秀良
|
Unravelling the {} Twin Intersection Between LPSO Structure/SFs in Magnesium Alloy
|
|
SHAO Xiaohong, PENG Zhenzhen, JIN Qianqian, MA Xiuliang
|
|
图6 LPSO结构间{}孪晶形核与相遇
|
Fig.6 High-magnification HAADF-STEM image of a region containing {} twin embryo and BB boundary between LPSO structure (insets I-V show the FFT images of regions I-V) (a), and atomic-resolution HAADF-STEM images showing the relatively wide overlapping due to the {} twin and matrix (b, c) (The yellow arrows in Figs.6b and c indicate propagation of the twin towards the matrix (PB—prismatic-basal)
|
|
|
|
|