GH4061合金在高压富氧环境下的燃烧行为 |
| 曹姝婷, 张少华, 张健 |
|
Combustion Behavior of GH4061 Alloy in High Pressure and Oxygen-Enriched Atmosphere |
| CAO Shuting, ZHANG Shaohua, ZHANG Jian |
| 图8 GH4061合金燃烧过程示意图 |
| Fig.8 Schematics of combustion process of GH4061 alloy (x1—thickness of melting zone, x2—thickness of oxide zone, T1—flame temperature, T2—combustion front temperature, T3—transition zone temperature) (a) combustion start (b) generation and movement of oxides (c) combustion stop |
|