GH4061合金在高压富氧环境下的燃烧行为 |
| 曹姝婷, 张少华, 张健 |
|
Combustion Behavior of GH4061 Alloy in High Pressure and Oxygen-Enriched Atmosphere |
| CAO Shuting, ZHANG Shaohua, ZHANG Jian |
| 图5 GH4061合金在7 MPa压强下燃烧后燃烧区域前端氧化物区形貌以及EDS元素分布 |
| Fig.5 Morphology and EDS elements distribution in oxide zone of combustion zone for GH4061 alloy after combustion at 7 MPa |
|