GH4061合金在高压富氧环境下的燃烧行为 |
| 曹姝婷, 张少华, 张健 |
|
Combustion Behavior of GH4061 Alloy in High Pressure and Oxygen-Enriched Atmosphere |
| CAO Shuting, ZHANG Shaohua, ZHANG Jian |
| 图4 GH4061合金在7 MPa压强下燃烧后燃烧区域的截面组织 |
| Fig.4 Cross sectional microstructures of combustion zone of GH4061 alloy after combustion at 7 MPa (a) original alloy, transition zone, and melting zone (b) fine dendrites in transition zone (c) melting zone |
|