GH4061合金在高压富氧环境下的燃烧行为 |
| 曹姝婷, 张少华, 张健 |
|
Combustion Behavior of GH4061 Alloy in High Pressure and Oxygen-Enriched Atmosphere |
| CAO Shuting, ZHANG Shaohua, ZHANG Jian |
| 图2 GH4061合金在实验压强为3.5 MPa时的燃烧过程 |
| Fig.2 High-speed camera images of combustion process of GH4061 alloy in 3.5 MPa PIC test (PIC—promoted ignition-combustion) (a, b) ignite the promoter (c-h) a burn-drop cycle (i-k) the end of burning |
|