中国科学院金属研究所冷喷涂技术研究进展 |
| 熊天英, 王吉强 |
|
Research Progress of Cold Spray in Institute of Metal Research, Chinese Academy of Sciences |
| XIONG Tianying, WANG Jiqiang |
| 图3 Cu/Zn颗粒界面的元素分布和高分辨透射电镜像[ |
| Fig.3 EDS mapping (a) and HRTEM image with fast fourier transform (FFT) patterns (insets) (b) of Cu/Zn particles' interface[ |
|