中国科学院金属研究所冷喷涂技术研究进展 |
| 熊天英, 王吉强 |
|
Research Progress of Cold Spray in Institute of Metal Research, Chinese Academy of Sciences |
| XIONG Tianying, WANG Jiqiang |
| 图2 316L不锈钢颗粒沉积在不同基体上的SEM像(喷涂参数:800℃,3.5 MPa)[ |
| Fig.2 SEM images of as-sprayed single 316L particles on pure Al (a), pure Cu (b), AISI1015 mild steel (c), 7075T6 Al alloy (d), Inconel625 (e), and Ti6Al4V (f) (Spray condition: 800oC, 3.5 MPa)[ |
|