以抗CMAS腐蚀为目标的稀土硅酸盐环境障涂层高熵化设计与性能提升 |
| 王京阳, 孙鲁超, 罗颐秀, 田志林, 任孝旻, 张洁 |
|
Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion |
| WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie |
| 图6 高熵稀土双硅酸盐(Er0.25Tm0.25Yb0.25Lu0.25)2Si2O7 1500℃ CMAS腐蚀机制示意图[ |
| Fig.6 Schematic diagrams for the interaction between CMAS and (Er0.25Tm0.25Yb0.25Lu0.25)2Si2O7 high-entropy disilicate at 1500oC[ |
|