以抗CMAS腐蚀为目标的稀土硅酸盐环境障涂层高熵化设计与性能提升 |
| 王京阳, 孙鲁超, 罗颐秀, 田志林, 任孝旻, 张洁 |
|
Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion |
| WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie |
| 图2 3类稀土单硅酸盐(RE2SiO5) 1300℃ CMAS腐蚀50 h反应示意图[ |
| Fig.2 Schematic diagrams of the performances of RE2SiO5 after CMAS corrosion at 1300oC for 50 h[ |
|