耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展
吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜

Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels
WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu
表1 ASS-Si奥氏体钢和Type 304奥氏体钢在550℃下的拉伸强度和持久强度 (MPa)
Table 1 Tensile and creep-rupture strength of Type 304 aus-tenitic steel and ASS-Si austenitic steel at 550oC
SteelYield strengthTensile strength3000 h creep-rupture strength

Type 304

ASS-Si

106

201

349

433

210

220