耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展
吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜

Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels
WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu
图6 9Cr-Si在550℃静态饱和氧LBE环境下腐蚀1000 h后的氧化层形貌及元素分布
Fig.6 Cross-sectional back scattered electron (BSE) image (a) and corresponding line scanning (b) of 9Cr-Si alloy after exposure for 1000 h to stagn-ant oxygen-saturated LBE at 550oC