耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展
吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜

Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels
WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu
图4 T91和316钢在高温空气与液态LBE环境中疲劳寿命对比
Fig.4 Comparisons between fatigue life in air and liquid LBE (ASME—America Society of Mechanical Engineers)
(a) T91 steel (b) 316 stainless steel