耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展
吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜

Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels
WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu
图2 铁素体/马氏体钢T91在550℃液态LBE中浸泡1000 h后的截面形貌[4]
Fig.2 Cross-section morphologies of oxide films on T91 steel after 1000 h exposure in liquid LBE at 550oC and different mass fractions of dissolved oxygen (DO)[4] (OOL—outer oxide layer, IOL—inner oxide layer, IOZ—inner oxide zone, OL—oxide layer)
(a) saturated oxygen (b) 1.26 × 10-6% DO (c) 1.41 × 10-8% DO (d) 1.12 × 10-9% DO