3D打印医用钛合金多孔材料力学性能研究进展
李述军, 侯文韬, 郝玉琳, 杨锐

Research Progress on the Mechanical Properties of the Biomedical Titanium Alloy Porous Structures Fabricated by 3D Printing Technique
LI Shujun, HOU Wentao, HAO Yulin, YANG Rui
图11 SEBM制备Ti2448和Ti-6Al-4V合金多孔材料的S-N曲线、归一化S-N曲线以及弹性模量与疲劳强度的关系[42]
Fig.11 S-N curves (a) and normalized S-N curves (b) of the porous Ti2448 and Ti-6Al-4V specimens with different porosities, and the relationship of elastic modulus and the fatigue strength for the SEBM porous Ti2448 and Ti-6Al-4V specimens (c)[42]