| 李述军, 侯文韬, 郝玉琳, 杨锐 |
|
Research Progress on the Mechanical Properties of the Biomedical Titanium Alloy Porous Structures Fabricated by 3D Printing Technique |
| LI Shujun, HOU Wentao, HAO Yulin, YANG Rui |
| 图7 选区电子束熔化(SEBM)制备Ti-6Al-4V合金多孔材料原始态和退火态的应力-应变曲线和S-N曲线[ |
| Fig.7 Compressive engineering stress-strain curves (Inset shows the whole stress-strain curves ) (a) and S-N curves (b) of the as-fabricated and annealed SEBM Ti-6Al-4V meshes[ |
|