金属材料的组织定制 |
| 李殿中, 王培 |
|
Tailoring Microstructures of Metals |
| LI Dianzhong, WANG Pei |
| 图4 M50钢疲劳试样中的裂纹萌生区域形貌及EDS |
| Fig.4 Morphology and EDS element mappings of crack initiation region in tension-compression fatigue specimens of M50 steel (a-c) (FGA—fine grain area) |
|