金属材料的组织定制 |
| 李殿中, 王培 |
|
Tailoring Microstructures of Metals |
| LI Dianzhong, WANG Pei |
| 图2 低氧稀土处理的双真空M50钢中夹杂物统计 |
| Fig.2 Inclusions in the M50 steel manufactured by vacuum induction melting (VIM) + vacuum arc remelting (VAR) and low-oxygen RE treatment |
|