基于机器学习的中厚板变形抗力模型建模与应用 |
| 冀秀梅, 侯美伶, 王龙, 刘玠, 高克伟 |
|
Modeling and Application of Deformation Resistance Model for Medium and Heavy Plate Based on Machine Learning |
| JI Xiumei, HOU Meiling, WANG Long, LIU Jie, GAO Kewei |
| 图7 Deep_RM和Deep_All预测值分别与RM真实值的偏差绝对值分布对比 |
| Fig.7 Comparisons of the distribution of the absolute value of the deviation between the true value of RM deformation resistance and the predicted value obtained by Deep_RM (a) and Deep_All (b) ( |
|