Y对无取向6.5%Si钢凝固组织、中温压缩变形和软化机制的影响 |
| 李民, 王继杰, 李昊泽, 邢炜伟, 刘德壮, 李奥迪, 马颖澈 |
|
Effect of Y on the Solidification Microstructure, Warm Compression Behavior, and Softening Mechanism of Non-Oriented 6.5%Si Electrical Steel |
| LI Min, WANG Jijie, LI Haoze, XING Weiwei, LIU Dezhuang, LI Aodi, MA Yingche |
| 图14 不同Y含量铸态试样500℃压缩后芯部晶粒的LM分布图和对应的几何必须位错(GND)密度 |
| Fig.14 LM distribution histograms of the as-cast 0Y (a), 0.017Y (b), and 0.15Y (c) samples after compression at 500oC, and the corresponding geometrically necessary dislocation (GND) densities (ρGND) (d) (R2—coefficient of determination) |
|