Y对无取向6.5%Si钢凝固组织、中温压缩变形和软化机制的影响 |
| 李民, 王继杰, 李昊泽, 邢炜伟, 刘德壮, 李奥迪, 马颖澈 |
|
Effect of Y on the Solidification Microstructure, Warm Compression Behavior, and Softening Mechanism of Non-Oriented 6.5%Si Electrical Steel |
| LI Min, WANG Jijie, LI Haoze, XING Weiwei, LIU Dezhuang, LI Aodi, MA Yingche |
| 图6 不同Y含量铸锭的XRD谱 |
| Fig.6 XRD spectra of the ingots with various Y contents |
|